Effect of distilled and sea water absorption on mechanical behaviour of short coir fibre epoxy composite/sawdust filler

Moorthy M. Nair, Nagaraja Shetty, S. Divakara Shetty, M. Shambhavi Kamath

Research output: Contribution to journalArticle

1 Citation (Scopus)

Abstract

Research on natural fibres has been carried out from past decades as a result of developing low cost, eco-friendly materials. The objective of this study is to fabricate composites utilising sawdust of various proportion and compare the mechanical properties like tensile, flexural and hardness within dry condition and with respect to specimens immersed in distilled and salt water. The composites with constant reinforcement 15%, different percentage of matrix (85, 80, 75, 70%) and filler (0, 5, 10, 15%), respectively by mass, are developed by hand layup method and is compared for their mechanical properties. Mechanical properties of composite fabricated from sawdust up to certain percentage showed an improvement when compared to composite with no filler; with further increase in filler, a drop in mechanical performance is noticed. An increase in tensile strength by 12.75%, flexural strength by 5.94%, hardness by 18.34%, tensile modulus by 100.3%, flexural modulus by 60.4% is observed in dry condition compared to the composite with no filler. Mechanical degradation in tensile strength, tensile modulus, hardness, flexural strength for the samples subjected to ageing in sea and distilled water is observed. Flexural modulus after ageing increased with filler addition up to a certain percentage and with further increase in filler, a decrease is noticed. Higher mechanical degradation (except flexural modulus) is observed for those specimens immersed in sea water.

Original languageEnglish
Pages (from-to)261-282
Number of pages22
JournalPertanika Journal of Science and Technology
Volume26
Issue number1
Publication statusPublished - 01-01-2018

Fingerprint

coir
filling materials
Sawdust
sawdust
composite materials
Hardness
Seawater
Water absorption
epoxides
Fillers
seawater
Tensile Strength
Fibers
Composite materials
hardness
mechanical property
mechanical properties
tensile strength
strength (mechanics)
Bending strength

All Science Journal Classification (ASJC) codes

  • Computer Science(all)
  • Chemical Engineering(all)
  • Environmental Science(all)
  • Agricultural and Biological Sciences(all)

Cite this

@article{66528237afdf409d95d10d4dca1e235e,
title = "Effect of distilled and sea water absorption on mechanical behaviour of short coir fibre epoxy composite/sawdust filler",
abstract = "Research on natural fibres has been carried out from past decades as a result of developing low cost, eco-friendly materials. The objective of this study is to fabricate composites utilising sawdust of various proportion and compare the mechanical properties like tensile, flexural and hardness within dry condition and with respect to specimens immersed in distilled and salt water. The composites with constant reinforcement 15{\%}, different percentage of matrix (85, 80, 75, 70{\%}) and filler (0, 5, 10, 15{\%}), respectively by mass, are developed by hand layup method and is compared for their mechanical properties. Mechanical properties of composite fabricated from sawdust up to certain percentage showed an improvement when compared to composite with no filler; with further increase in filler, a drop in mechanical performance is noticed. An increase in tensile strength by 12.75{\%}, flexural strength by 5.94{\%}, hardness by 18.34{\%}, tensile modulus by 100.3{\%}, flexural modulus by 60.4{\%} is observed in dry condition compared to the composite with no filler. Mechanical degradation in tensile strength, tensile modulus, hardness, flexural strength for the samples subjected to ageing in sea and distilled water is observed. Flexural modulus after ageing increased with filler addition up to a certain percentage and with further increase in filler, a decrease is noticed. Higher mechanical degradation (except flexural modulus) is observed for those specimens immersed in sea water.",
author = "Nair, {Moorthy M.} and Nagaraja Shetty and {Divakara Shetty}, S. and {Shambhavi Kamath}, M.",
year = "2018",
month = "1",
day = "1",
language = "English",
volume = "26",
pages = "261--282",
journal = "Pertanika Journal of Science and Technology",
issn = "0128-7680",
publisher = "Universiti Putra Malaysia",
number = "1",

}

Effect of distilled and sea water absorption on mechanical behaviour of short coir fibre epoxy composite/sawdust filler. / Nair, Moorthy M.; Shetty, Nagaraja; Divakara Shetty, S.; Shambhavi Kamath, M.

In: Pertanika Journal of Science and Technology, Vol. 26, No. 1, 01.01.2018, p. 261-282.

Research output: Contribution to journalArticle

TY - JOUR

T1 - Effect of distilled and sea water absorption on mechanical behaviour of short coir fibre epoxy composite/sawdust filler

AU - Nair, Moorthy M.

AU - Shetty, Nagaraja

AU - Divakara Shetty, S.

AU - Shambhavi Kamath, M.

PY - 2018/1/1

Y1 - 2018/1/1

N2 - Research on natural fibres has been carried out from past decades as a result of developing low cost, eco-friendly materials. The objective of this study is to fabricate composites utilising sawdust of various proportion and compare the mechanical properties like tensile, flexural and hardness within dry condition and with respect to specimens immersed in distilled and salt water. The composites with constant reinforcement 15%, different percentage of matrix (85, 80, 75, 70%) and filler (0, 5, 10, 15%), respectively by mass, are developed by hand layup method and is compared for their mechanical properties. Mechanical properties of composite fabricated from sawdust up to certain percentage showed an improvement when compared to composite with no filler; with further increase in filler, a drop in mechanical performance is noticed. An increase in tensile strength by 12.75%, flexural strength by 5.94%, hardness by 18.34%, tensile modulus by 100.3%, flexural modulus by 60.4% is observed in dry condition compared to the composite with no filler. Mechanical degradation in tensile strength, tensile modulus, hardness, flexural strength for the samples subjected to ageing in sea and distilled water is observed. Flexural modulus after ageing increased with filler addition up to a certain percentage and with further increase in filler, a decrease is noticed. Higher mechanical degradation (except flexural modulus) is observed for those specimens immersed in sea water.

AB - Research on natural fibres has been carried out from past decades as a result of developing low cost, eco-friendly materials. The objective of this study is to fabricate composites utilising sawdust of various proportion and compare the mechanical properties like tensile, flexural and hardness within dry condition and with respect to specimens immersed in distilled and salt water. The composites with constant reinforcement 15%, different percentage of matrix (85, 80, 75, 70%) and filler (0, 5, 10, 15%), respectively by mass, are developed by hand layup method and is compared for their mechanical properties. Mechanical properties of composite fabricated from sawdust up to certain percentage showed an improvement when compared to composite with no filler; with further increase in filler, a drop in mechanical performance is noticed. An increase in tensile strength by 12.75%, flexural strength by 5.94%, hardness by 18.34%, tensile modulus by 100.3%, flexural modulus by 60.4% is observed in dry condition compared to the composite with no filler. Mechanical degradation in tensile strength, tensile modulus, hardness, flexural strength for the samples subjected to ageing in sea and distilled water is observed. Flexural modulus after ageing increased with filler addition up to a certain percentage and with further increase in filler, a decrease is noticed. Higher mechanical degradation (except flexural modulus) is observed for those specimens immersed in sea water.

UR - http://www.scopus.com/inward/record.url?scp=85041074461&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=85041074461&partnerID=8YFLogxK

M3 - Article

AN - SCOPUS:85041074461

VL - 26

SP - 261

EP - 282

JO - Pertanika Journal of Science and Technology

JF - Pertanika Journal of Science and Technology

SN - 0128-7680

IS - 1

ER -