Tensile fractography of artificially aged al6061-sic+b4c hybrid composites

Research output: Chapter in Book/Report/Conference proceedingConference contribution

1 Citation (Scopus)

Fingerprint

Dive into the research topics of 'Tensile fractography of artificially aged al6061-sic+b4c hybrid composites'. Together they form a unique fingerprint.

Physics & Astronomy

Engineering & Materials Science

Chemical Compounds